Thursday, 14 August 2014

. Chemically set bricks


Chemically set bricks are not fired but may have the curing process accelerated by the application of heat and pressure in an autoclave.

Calcium-silicate bricks


Swedish Mexitegel.
Calcium silicate bricks are also called sandlime or flintlime bricks depending on their ingredients. Rather than being made with clay they are made with lime binding the silicate material. The raw materials for calcium-silicate bricks include lime mixed in a proportion of about 1 to 10 with sand, quartz, crushed flint or crushed siliceous rock together with mineral colourants. The materials are mixed and left until the lime is completely hydrated; the mixture is then pressed into moulds and cured in an autoclave for three to fourteen hours to speed the chemical hardening.[17] The finished bricks are very accurate and uniform, although the sharp arrises need careful handling to avoid damage to brick and bricklayer. The bricks can be made in a variety of colours; white, black, buff and grey-blues are common and pastel shades can be achieved. This type of brick is common in Sweden, especially in houses built or renovated in the 1970s, where it is known as "Mexitegel" (en: Mexi[can] Bricks). In India these are known as fly ash bricks, manufactured using the FaL-G (fly ash, lime and gypsum) process. Calcium-silicate bricks are also manufactured in Canada and the United States, and meet the criteria set forth in ASTM C73 – 10 Standard Specification for Calcium Silicate Brick (Sand-Lime Brick). It has lower embodied energy than cement based man-made stone and clay brick.[citation needed]

Concrete bricks



A concrete brick-making assembly line in Guilinyang Town, Hainan, China. This operation produces a pallet containing 42 bricks, approximately every 30 seconds.
Bricks of concrete with sand aggregate can be made using a simple machine and a basic assembly line. A conveyor belt adds the mixture to a machine, which pours a measured amount of concrete into a form. The form is vibrated to remove bubbles, after which it is raised to reveal the wet bricks, spaced out on a plywood sheet. A small elevator then stacks these palettes, after which a forklift operator moves them to the brickyard for drying.
Concrete bricks are available in many colours and as an engineering brick made with sulfate-resisting Portland cement or equivalent. When made with adequate amount of cement they are suitable for harsh environments such as wet conditions and retaining walls. They are made to standards BS 6073, EN 771-3. Concrete bricks expand and contract more than clay or sandlime bricks so they need movement joints every 5 to 6 metres, but are similar to other bricks of similar density in thermal and sound resistance and fire resistance.[

Methods of manufacture



Brick making at the beginning of the 20th century.
Three basic types of brick are un-fired, fired, and chemically set bricks. Each type is manufactured differently.

Fired brick

Fired bricks are burned in a kiln which makes them durable. Modern, fired, clay bricks are formed in one of three processes – soft mud, dry press, or extruded.
Normally, brick contains the following ingredients:[15]
  1. Silica (sand) – 50% to 60% by weight
  2. Alumina (clay) – 20% to 30% by weight
  3. Lime – 2 to 5% by weight
  4. Iron oxide – ≤ 7% by weight
  5. Magnesia – less than 1% by weight
The soft mud method is the most common, as it is the most economical. It starts with the raw clay, preferably in a mix with 25–30% sand to reduce shrinkage. The clay is first ground and mixed with water to the desired consistency. The clay is then pressed into steel moulds with a hydraulic press. The shaped clay is then fired ("burned") at 900–1000 °C to achieve strength.

Rail kilns


Xhosa brickmaker at kiln near Ngcobo in the former Transkei in 2007.
In modern brickworks, this is usually done in a continuously fired tunnel kiln, in which the bricks are fired as they move slowly through the kiln on conveyors, rails, or kiln cars, which achieves a more consistent brick product. The bricks often have lime, ash, and organic matter added, which accelerates the burning process.

Bull's Trench Kilns

In India, brick making is typically a manual process. The most common type of brick kiln in use there is the Bull's Trench Kiln (BTK), based on a design developed by British engineer W. Bull in the late 19th century.
An oval or circular trench is dug, 6–9 metres wide, 2-2.5 metres deep, and 100–150 metres in circumference. A tall exhaust chimney is constructed in the centre. Half or more of the trench is filled with "green" (unfired) bricks which are stacked in an open lattice pattern to allow airflow. The lattice is capped with a roofing layer of finished brick.
In operation, new green bricks, along with roofing bricks, are stacked at one end of the brick pile; cooled finished bricks are removed from the other end for transport to their destinations. In the middle, the brick workers create a firing zone by dropping fuel (coal, wood, oil, debris, and so on) through access holes in the roof above the trench.

West face of Roskilde Cathedral in Roskilde, Denmark.
The advantage of the BTK design is a much greater energy efficiency compared with clamp or scove kilns. Sheet metal or boards are used to route the airflow through the brick lattice so that fresh air flows first through the recently burned bricks, heating the air, then through the active burning zone. The air continues through the green brick zone (pre-heating and drying the bricks), and finally out the chimney, where the rising gases create suction which pulls air through the system. The reuse of heated air yields savings in fuel cost.
As with the rail process above, the BTK process is continuous. A half dozen labourers working around the clock can fire approximately 15,000–25,000 bricks a day. Unlike the rail process, in the BTK process the bricks do not move. Instead, the locations at which the bricks are loaded, fired, and unloaded gradually rotate through the trench.[16]

Dry pressed bricks

The dry press method is similar to the soft mud brick method, but starts with a much thicker clay mix, so it forms more accurate, sharper-edged bricks. The greater force in pressing and the longer burn make this method more expensive.

Extruded bricks

For extruded bricks the clay is mixed with 10–15% water (stiff extrusion) or 20–25% water (soft extrusion) in a pugmill. This mixture is forced through a die to create a long cable of material of the desired width and depth. This mass is then cut into bricks of the desired length by a wall of wires. Most structural bricks are made by this method as it produces hard, dense bricks, and suitable dies can produce perforations as well. The introduction of such holes reduces the volume of clay needed, and hence the cost. Hollow bricks are lighter and easier to handle, and have different thermal properties from solid bricks. The cut bricks are hardened by drying for 20 to 40 hours at 50 to 150 °C before being fired. The heat for drying is often waste heat from the kiln.
European-style extruded bricks or blocks are used in single-wall construction with finishes applied on the inside and outside. Their many voids comprise a greater proportion of the volume than the solid, thin walls of fired clay. Such bricks are made in 15-, 25-, 30-, 42- and 50-cm widths. Some models have very high thermal insulation properties, making them suitable for zero-energy buildings.

Types of fired clay bricks

There are thousands of types of bricks that are named for their use, size, forming method, origin, quality, texture, and/or materials.
  • Face - A very common classification meaning they are suitable to be visible.
  • Common or building - An less common type of brick not intended to be visible such as being underground or covered with render or plaster.
  • Hollow - not solid, the holes are less than 25% of the brick volume
  • Perforated - holes greater than 25% of the brick volume
  • Indentations called frogs
  • Keyed - indentations in at least one face and end to be used with rendering and plastering
  • Paving - brick intended to be in ground contact as a walkway or roadway.
  • Ceramic glazed - face bricks with a decorative glazing
  • Thin - brick with normal height and length but thin width to be used as a veneer.
  • Chemically resistant -
  • Industrial floor -
  • Engineering - a type of hard, dense, brick used where strength, low water porosity or acid (flue gas) resistance are needed. Further classified as type A and type B based on their compressive strength.
  • accrington - a type of engineering brick
  • Acid brick - acid resistant bricks
  • Fire or refractory - highly heat resistant bricks
  • Clinker - a vitrified brick
  • Salmon - an under burned brick, soft and porous named for its color
  • Dutch -
  • Roman -
  • Norman -
  • Cream City brick - a light yellow brick made in Milwaukee, Wisconsin
  • London stock -
  • Staffordshire blue brick -
  • Fareham red brick -
  • Nanak Shahi bricks - a type of brick in India
  • Wire cut - cut to size with a tensioned wire which may leave drag marks
  • Water struck - the mould is dipped in water before forming the brick giving the brick an irregular texture when the mould is removed
  • Sand struck - hand made in a mould coated with sand
  • Sand surfaced -
  • Flashed - heated to produce a deeper color on the face and end
  • numerous other textures including smooth, velour, matte, sandblasted, bark...
  • Extruded - made by being forced through an opening, a very consistent size and shape.
  • Pressed - wire cut bricks which are then pressed to improve appearances
  • Moulded - shaped in moulds rather than being extruded
  • Interior quality - lower quality brick not for exterior exposure
  • Special quality - High quality for use in wet and freezing conditions
  • BS 3921 classifies the soluble salt content grades as L (low) and N (normal), frost resistance as F (frost resistant), M (moderately frost resistant), or O (not-frost resistant, for internal use only). These class can be combined such as a type LF brick has a low salt content and is frost resistant.